[Elsevier] Removing loose oxide layer and producing dense α-phase layer simultaneously to improve corrosion resistance of Ti-6Al-4V titanium alloy by coupling electrical pulse and ultrasonic treatment

zxx0502 Post time 2024-6-4 13:46:48 | Show all posts |Read mode
Reward10points

通过电脉冲和超声波处理耦合,去除松散的氧化层并同时产生致密的α相层,以提高Ti-6Al-4V钛合金的耐腐蚀性

表面和涂层技术
[size=0.7]卷 384,25二月2020,125329